Author |
Message |
Ralph Liebing, RA, CSI, CDT Senior Member Username: rliebing
Post Number: 1358 Registered: 02-2003
| Posted on Tuesday, December 04, 2012 - 11:37 am: | |
How do you approach/specify welding of the inside [concealed] side of SS frame joints? Is there a standard for this? |
Margaret G. Chewning FCSI CCS Senior Member Username: presbspec
Post Number: 227 Registered: 01-2003
| Posted on Tuesday, December 04, 2012 - 11:54 am: | |
Welding standard for SS is AWS D1.6. As far as the finish goes, I require "Grind exposed joints flush and smooth with adjacent finish surface." |
ken hercenberg Senior Member Username: khercenberg
Post Number: 385 Registered: 12-2006
| Posted on Tuesday, December 04, 2012 - 12:44 pm: | |
Check out the HMMA standard for stainless steel hollow metal doors and frames. http://www.naamm.org/landing_pages/HMMA_866-12.htm |